CAVOREN WPSAWS D1.1 WPS preparation

Completed documents · evidence explained

WPS examples and supporting working records

See how inputs become a complete procedure, then use the matching guides and working files for your own project. Each example explains where its values come from.

Prequalified route: A36 with SMAW

The complete A36 SMAW WPS demonstration adapts a published structural-steel procedure and provides Word, PDF and HTML files. Read the stated source and assumptions before comparing it with your joint.

Start with the A36 material and thickness guide, check the CJP joint-detail requirements, and collect your own facts in the WPS project intake checklist.

For a supported project, see the $299 prequalified WPS preparation service and its required inputs.

Existing-PQR route: a GMAW-S teaching case

The synthetic GMAW-S PQR-to-WPS case separates recorded test inputs, derived support and selected production ranges. Download the complete teaching WPS and derivation record. No welding or tests occurred for this teaching case.

Read why GMAW-S needs a qualification route, review PQR essential-variable evidence, and use the editable PQR coverage matrix to trace an actual record.

If your valid, applicable existing PQR covers the target, see the $499 existing-PQR WPS preparation service.

Use your own records before issuing a WPS

Use the PQR source record log for actual test evidence, the pass-level weld parameter record for actual observations, and the WPS technical review checklist to close required gaps.

The demonstrations do not provide project qualification evidence. The code edition and coverage page explains the basis used here; new qualification testing is outside the preparation service.