01 · COLLECT
WPS project intake checklist
Gather contract basis, joint geometry, two-sided base-metal details, process conditions and existing records. Includes a gap log that keeps unknown facts visible.
Open guideORIGINAL WORKING RESOURCES · AWS D1.1 WPS
Collect project facts, draft a production procedure from a confirmed technical basis, and trace PQR coverage with separate evidence and range fields.
01 · COLLECT
Gather contract basis, joint geometry, two-sided base-metal details, process conditions and existing records. Includes a gap log that keeps unknown facts visible.
Open guide02 · DRAFT
Organize scope, joint preparation, consumables, process schedule, temperature controls and document approvals. Select one supported qualification basis.
Open guide03 · TRACE
Link each PQR and process segment to actual record values, the applicable support basis and the final WPS production range.
Open guide04 · SOURCE
Transcribe actual PQR facts by process segment, link test evidence, and keep derived production coverage in separate fields.
Open guide05 · RECORD
Capture parameters by pass while separating actual PQR or trial observations from proposed WPS settings and supported ranges.
Open guide06 · REVIEW
Review route-specific evidence, separate accepted findings from unresolved gaps, and apply a clear issue gate.
Open guideRead the WPS knowledge paths to choose which record you need. The completed WPS examples show published-source and synthetic teaching inputs separately.
For project-specific preparation, review the inputs for prequalified WPS preparation · $299 or preparation from an applicable existing PQR · $499.